Butt Fusion welding checklist

Butt Fusion welding checklist
  • Trim the pipe ends all the way around
  • Clean the heater plates
  • When clamping the pipes in place, use the clamps to re-round the pipes
  • Correct procedure: Ask for evidence of recent, random weld inspections by your supervisors

Pressure

  1. Measure the drag pressure
  2. Check the right fusion pressure
  3. Add the two together for the overall pressure setting

Temperature

  1. Set the right heater place temperature (usually in the reange of 200-240C
  2. Give enough heat soak time for the pipe ends to fully heat up
  3. Keep dwell time down so the pipe ends don’t cool before contact

Alighnment

  1. Aim for less than 1mm misalignment
  2. For thicker pipes, misalignment must not exceed 10% of the pipe wall thickness (e.g. for 18mm thick pipe, no more thatn 1.8mm)

When you need focused help fast, get it from a supplier whose success is
keeping your plant moving. Call Advanced Piping Systems now on 1300 792 879

Related Articles

APS Electrofusion Jointing Guide

Electrofusion Welding

Tips for systematic preparation for successful electrofusion jointing Know your stuff Get the right training and industry accreditation. A methodical approach in the preparation and …

The smartest way to speed up your upgrade from steel to poly pipe

Prefabrication

Using your existing maintenance program, combined with a plan of what you want to achieve, is the simplest place to start. By speaking to a …

Eliminate risk and reduce your downtime – critical factors to consider to eliminate pipe deflection stress

Training

Can the right support prevent your pipeline’s shutdown? n polyethylene pipelines, insufficient supports and bracketing can lead to unwanted shutdowns because it causes further problems. …

Don’t get caught out: the benefits of catch pits

Training Fittings

Across the globe, catch pits play a vital role in wastewater and water management systems, with benefits including helping to prevent costly blockages, flooding and …